Skip to main content

Table 10 Test results after deformation by stretching at a temperature of 600 °C of steel 10XN3MD

From: Study of the sensitivity of high-strength cold-resistant shipbuilding steels to thermal cycle of arc welding

 

Time before failure, s

Elongation for 15 mm base, %

Base metal

23,070

14

Imitation of the HAZ region

4970

1