Skip to main content

Table 1 The electrolytes prepared based on three different conditions

From: Structural studies of NiTe2 thin films with the influence of amino additives

Electrolyte

Without additive

With EDTA

With TEA

Molarity (M)

0.015 NiSO4·6H2O + 0.003 TeO2

0.015 NiSO4·6H2O + 0.003 TeO2 + 0.053

0.015 NiSO4·6H2O + 0.003 TeO2 +

Composition of additive

-

0.053 M EDTA

1.0 M TEA

Acidic/basic condition

Base (pH 10)

Acidic (pH 3)

Base (pH 10)

  1. Sources: Aricò et al. 1997; Saloniemi et al. 1998; Takahashi et al. 1994.