From: Structural properties of batch foamed acrylonitrile butadiene styrene/nanoclay nanocomposites
Parameter | f | s | v | P% |
---|---|---|---|---|
Nanoclay percentage | 2 | 23.4 × 10−3 | 11.7 × 10−3 | 15 |
Saturation pressure | 2 | 33 × 10−3 | 16.5 × 10−3 | 21 |
Foaming temperature | 2 | 85.9 × 10−3 | 42.95 × 10−3 | 55 |
Foaming time | 2 | 14.3 × 10−3 | 7.15 × 10−3 | 9 |
Pooled error | 0 | 0 | 0 | – |
Total | 8 | 156.6 × 10−3 | – | 100 |