Fig. 1From: The environment-induced cracking of as-annealed Ni3(Si,Ti) and Ni3(Si,Ti) with 2Mo in sodium chloride solutionsCorrosion elongation curve of as-annealed Ni3(Si,Ti) at 1000 MPa and as-annealed Ni3(Si,Ti) + 2Mo at 1450 MPa in 0.5 kmol/m3 NaCl solution at 313 K. t f time to failure, l ss steady-state elongation rate, t ss transition timeBack to article page