Fig. 3From: The environment-induced cracking of as-annealed Ni3(Si,Ti) and Ni3(Si,Ti) with 2Mo in sodium chloride solutionsThe relationships between applied stress and steady-state elongation rate in 0.5Â kmol/m3 NaCl solution at 313Â K. Ni3(Si,Ti) (black square). Ni3(Si,Ti)with 2Mo (circle)Back to article page