Fig. 6From: The environment-induced cracking of as-annealed Ni3(Si,Ti) and Ni3(Si,Ti) with 2Mo in sodium chloride solutionsThe relationships between steady-state elongation rate and a reciprocal of test temperature measured in 0.5Â kmol/m3 NaCl solution. Ni3(Si,Ti) at a constant applied stress of 1000Â MPa (black square). Ni3(Si,Ti) with 2Mo at a constant applied stress 1450Â MPa (circle)Back to article page