From: Influence of the holding time of the deep cryogenic treatment on the strain hardening behavior of HY-TUF steel
C
Mn
Si
Ni
Co
Cr
Mo
V
Cu
Al
Ti
Fe
Ms (°C)
0.25
1.40
1.60
1.80
–
0.30
0.45
Balance
357