Table 5 L9 orthogonal array followed for wear analysis

From: Synthesis and characterisation of hot extruded aluminium-based MMC developed by powder metallurgy route

Run

Load (N)

Track dia (mm)

RPM of counter disc

1

20

50

200

2

20

70

400

3

20

90

600

4

40

50

400

5

40

70

600

6

40

90

200

7

60

50

600

8

60

70

200

9

60

90

400