Fig. 13From: High cycle fatigue and fatigue crack propagation behaviors of β-annealed Ti-6Al-4V alloyThe SEM fractographs of β-annealed Ti64 specimen, FCP tested at an R ratio of 0.7 and documented at (a) ΔKth regime and (b) the ΔK of 30 MPa√mBack to article page