Table 3 Idem for and ASTM A 514 grade S

From: Effect of torch process on the steels used for bucket, shovel handle, and other high-tonne mining equipment

Relative position

(see text) (mm)

ASTM 514

(HV)

0.5

285

1

246

1.5

216

2.0

236

2.5

257

3.0

245

3.5

242

4.0

243

4.5

253

5.0

249

5.5

251

6.0

250

7.0

260