From: Study of the sensitivity of high-strength cold-resistant shipbuilding steels to thermal cycle of arc welding

Fig. 4

The structure (a, b, d, e) and fracture (c, f) of the base metal 10XN3MD after tempering 600 °C (a) and simulated on Gleeble-3800 coarse-grained region of the HAZ and of steel 10XN3MDF after heating to 600 °C and tempering 1350 °C (g) and after deformation at a speed 5.5 × 10− 6 s− 1 at a temperature of 600 °C (b, c, e, f), the base metal (b, c), and the coarse-grained region (d, f)