Table 8 Results of the surface roughness variance analysis for the second test

From: The effect of alumina powder in dielectric on electrical discharge machining parameters of aluminum composite A413-Al2O3 by the Taguchi method, the signal-to-noise analysis and the total normalized quality loss

Parameter

Degrees of freedom

(DF)

Sum of squares

(SS)

Mean of squares

(MS)

F value

P value

Degree of impact

(rank)

Voltage

1

4.311

4.311

4.293

0.0770

2

Current

2

65.667

32.833

22.059

0.0017

1

Pulse-on time

2

1.350

0.675

0.553

0.6021

4

Pulse-off time

2

3.271

1.636

4.385

0.3224

3