Table 4 The experimental LCCs for multi-cracked specimens with vertical cracks alignment (Fig. 2c)

From: Ductile failure analysis of epoxy resin plates containing multiple circular arc cracks by means of the equivalent material concept

2β(deg.)

P1 (N)

P2 (N)

P3 (N)

Pavg (N)

  

2a/d = 0.9

  

40

1805

1713

1860

1793

80

1887

1943

1991

1939

120

2054

2105

2204

2121

160

2241

2380

2493

2371

  

2a/d = 0.6

  

40

1753

1939

1861

1851

80

1909

2099

2047

1949

120

2196

2150

2290

2203

160

2332

2451

2405

2395