Skip to main content

Table 1 The tensile properties of β-annealed and mill-annealed Ti64 specimens

From: High cycle fatigue and fatigue crack propagation behaviors of β-annealed Ti-6Al-4V alloy

Heat treatment

YS (MPa)

UTS (MPa)

Tensile Elongation (%)

β-annealing

867

950

4.2

Mill-annealing

953

979

18.0