Table 2 Material parameters [MPa] for the Neo-Hookean and Mooney-Rivlin hyper-elastic models

From: Non-contact experimental methods to characterise the response of a hyper-elastic membrane

 

Neo-Hookean model

Mooney-Rivlin model

Sample

C 1

C 10

C 20

1

0.797

0.140

0.806

2

0.764

0.193

0.701

3

0.825

0.152

0.829

4

0.800

0.131

0.823

5

0.768

0.142

0.767

Average

0.791

0.152

0.785