From: Study of the sensitivity of high-strength cold-resistant shipbuilding steels to thermal cycle of arc welding
Steel grade
Tensile strength, MPa
Yield strength, MPa
Elongation, %
Reduction of area, %
09G2FB
≥ 550
≥ 430
≥ 20
–
10XN2MD
≥ 750
≥ 700
≥ 19
≥ 73
08XN3MD
≥ 600
≥ 18
12XN3MF
≥ 588
≥ 637
≥ 55