Fig. 2From: Sintering driving force of Al2O3 powders at the initial stage of pulse electric current sintering under thermoelastic diffusionTemperature distribution. a t = 4.2e−5 s, section xoy temperature distribution. b t = 4.5e−5 s, section xoy temperature distributionBack to article page