Table 2 The experimental LCCs for multi-cracked specimens with horizontal cracks alignment (Fig. 2a)

From: Ductile failure analysis of epoxy resin plates containing multiple circular arc cracks by means of the equivalent material concept

2β(deg.)

P1 (N)

P2 (N)

P3 (N)

Pavg (N)

  

2a/d = 0.9

  

40

1651

1742

1593

1663

80

1754

1793

1846

1797

120

1886

2042

1943

1958

160

2264

1924

2089

2092

  

2a/d = 0.6

  

40

1715

1870

1774

1786

80

1908

2023

1932

1954

120

2184

2063

2297

2181

160

2305

2363

2445

2372